MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Carmel Olefins CARMELCLEAR™ ME 74 E Specialty Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer; Polypropylene, Impact Modified; Molded/Extruded

Material Notes: CARMELCLEAR™ ME 74 E is a modified random polypropylene copolymer developed for extrusion of high impact transparent articles. It exhibits excellent impact resistance at low and ambient temperatures, very good transparency combined with good flexibility, low stress-whitening, and soft touch.

APPLICATIONS

CARMELCLEAR™ ME 74 E is suitable for flexible high-impact sheets, flexible lids with tight closure properties, films with low haze. Frequently it is used as impact modifier in blends with random copolymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 2.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
2.5 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Flexural Modulus 0.900 GPa131 ksiASTM D790
Izod Impact, Notched  0.300 J/cm
@Temperature >=-20.0 °C
0.562 ft-lb/in
@Temperature >=-4.00 °F
ASTM D256
 0.750 J/cm
@Temperature >=0.000 °C
1.41 ft-lb/in
@Temperature >=32.0 °F
ASTM D256
 5.00 J/cm
@Temperature >=23.0 °C
9.37 ft-lb/in
@Temperature >=73.4 °F
ASTM D256
 
Optical PropertiesMetricEnglishComments
Haze 32 %
@Thickness 1.60 mm
32 %
@Thickness 0.0630 in
plaque; ASTM D1003
Transmission, Visible 90 %90 %clear; thickness not quantified

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem FL31 LLDPE Cast Film Extrusion Polyethylene Copolymer
A. Schulman Diamond NPP10-0218 Low Density Polyethylene
Braskem TS9002 LDPE Blown Film Extrusion Polyethylene
Braskem LL4800N PEBDL Cast Film Extrusion Polyethylene Copolymer
Chevron Phillips MarFlex® HHM TR-258 Low Density Linear Polyethylene, Blown Film

PCARM037 / 79775

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.