MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Park Aerospace Nelco® NY9217 PTFE Laminate, Woven-Glass Reinforced
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminate system the material of choice for lowest loss, high frequency applications.

Key Features and Benefits:

  • Complete spectrum of controlled dielectric constants
  • Enhanced N9000 IM materials available
  • Consistent Quality
  • Optimized N9000 PTFE processing

Applications/Qualifications:

  • Cellular Base Station Antennas
  • Wireless Communications
  • Power Amplifiers
  • Dual Band Hi Power Passive Circuits
  • Automotive Applications
  • Digital/Microwave Hybrid Multilayer PCB Assemblies
  • Millimeter Wave Components
  • Telecommunications

Information provided by Park Electrochemical Corp.

Key Words: PTFE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.23 g/ccASTM D792A
Water Absorption <= 0.020 %IPC-TM-650.2.6.2.1
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 68.9 MPaCrosswise; IPC-TM-650.2.4.4
 82.7 MPaLengthwise; IPC-TM-650.2.4.4
Peel Strength 13.19 pliafter thermal shock (30 sec. at 260°C); IPC-TM-650.2.4.8
 13.3 pli18, 35, and 70µm copper; IPC-TM-650.2.4.8
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIPC-TM-650.2.5.17
Surface Resistance 1.00e+13 ohmIPC-TM-650.2.5.17
Dielectric Constant 2.15 - 2.19
@Frequency 1e+10 Hz
IPC-TM-650.2.5.5.5
Dielectric Breakdown 50000 VIPC-TM-650.2.5.6
Dissipation Factor 0.00080
@Frequency 1e+10 Hz
IPC-TM-650.2.5.5.5
Arc Resistance 180 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.9 µin/in-°FX; IPC-TM-650.2.4.41
 19.46 µin/in-°FY; IPC-TM-650.2.4.41
 144.56 µin/in-°FZ; IPC-TM-650.2.4.41
Thermal Conductivity 1.89 BTU-in/hr-ft²-°FASTM E1225
Flammability, UL94 V-0IPC-TM-650.2.3.10
 
Descriptive Properties
Passive Intermodulation Formulation AvailabilityYes
Passive Intermodulation Performance (dBc)-155

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Park Aerospace Nelco® NY9208 PTFE Laminate, Woven-Glass Reinforced
Park Aerospace Nelco® NY9220 PTFE Laminate, Woven-Glass Reinforced
Park Aerospace Nelco® NX9300 PTFE Laminate, Woven-Glass Reinforced
Park Aerospace Nelco® NY9233 PTFE Laminate, Woven-Glass Reinforced
Park Aerospace Nelco® NX9320 PTFE Laminate, Woven-Glass Reinforced

PPARK082 / 89354

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.