MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SAE 950X HSLA Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel

Material Notes: Treated with Nb or V. Better weldability and formability than HSLA grade 950C.

Key Words: High Strength Low Alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.75 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 438 MPaas rolled
Tensile Strength, Yield 339 MPaas rolled
Reduction of Area 64 %as rolled
Modulus of Elasticity 206 GPa
Bulk Modulus 163 GPaEstimated from elastic modulus
Poissons Ratio 0.29Typical for steel
Shear Modulus 80.0 GPaEstimated from elastic modulus
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.23 %
Iron, Fe >= 97.4 %As Balance
Manganese, Mn <= 1.35 %
Phosphorus, P <= 0.040 %
Silicon, Si <= 0.90 %
Sulfur, S <= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SAE 950A HSLA Steel
SAE 950D HSLA Steel, Composition Spec
SAE 950B HSLA Steel
SAE 950C HSLA Steel
AISI 1078 Steel, Hot Rolled Bar (UNS G10780)

MSSAE950X / 147607

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.