MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Nouryon Berolamine 1210 (BA-1210) Higher polyamine blend
Categories: Other Engineering Material

Material Notes: Berolamine-1210 (BA-1210) is a blend of higher polyethylene polyamines (isomers of TETA, TEPA, PEHA, and higher) and alkanolamines (AEEA, DEA, Hydroxyethyl DETA, and higher). BA-1210 is used as an intermediate in the manufacture of asphalt additives and epoxy curing agent.

CAS number: 84238-53-9 and 68910-05-4

EINECS/ELINCS No.: 282-508-4 and 272-729-4

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.024 g/cc0.03699 lb/in³
pH 121225% solution
Viscosity 40 cP40 cPDynamic viscosity
Vapor Pressure 9.00e-8 bar0.0000675 torr
 
Thermal PropertiesMetricEnglishComments
Melting Point <= -30.0 °C
@Pressure 0.1013 MPa
<= -22.0 °F
@Pressure 14.69 psi
Boiling Point 254 °C
@Pressure 0.1013 MPa
489 °F
@Pressure 14.69 psi
Flash Point 176 °C
@Pressure 0.1013 MPa
349 °F
@Pressure 14.69 psi
ISO 2719
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 10<= 10
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 1.0 %<= 1.0 %
 
Descriptive Properties
Amine number1200-1400 mg KOH/g
AppearanceYellowish brown
OdorAmmonical
Partition coefficient-2,6N-octanol/water, 25°C, log Pow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY430 / 285953

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.