MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lubrizol ESTANE® 58142 Ester Based Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Features: Fast cycling, broad temperature performance, and durability

Use: Injection Molding

Available in Americas, Europe, Middle East, Africa, India and Asia

Information provided by Lubrizol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.23 g/ccASTM D792
Maximum Moisture Content 0.020
Linear Mold Shrinkage 0.0070 cm/cmflex bar, Injection
 0.0080 cm/cmdisk, Injection
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 57 - 63
@Time 5.00 sec
ASTM D2240
Tensile Strength 38.0 MPaASTM D412
Elongation at Break 430 %ASTM D412
100% Modulus 0.0190 GPa
@Strain 100 %
ASTM D412
300% Modulus 0.0290 GPa
@Strain 300 %
ASTM D412
Flexural Modulus 34000 psiASTM D790
Tear Strength 290 pliASTM D470
Graves Tear Strength 1100 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 82CS-17, 1000g; ASTM D3389 B
Compression Set 34 %
@Temperature 23.0 °C,
Time 79200 sec
ASTM D395
 53 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Melting Point 212 °CDSC
Glass Transition Temp, Tg -24.0 °CDSC
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 210 °CInjection
 224 °CInjection
Middle Barrel Temperature 215 °CInjection
Nozzle Temperature 229 °CInjection
Melt Temperature 229 °CInjection
Drying Temperature 104 °C
Dry Time 2.00 - 4.00 hour
Dew Point -40.0 °C
Injection Pressure 10000 - 15000 psiInjection
Hold Pressure 5000 - 10000 psiInjection
Back Pressure >= 50.0 psiInjection
Screw Speed 60 - 100 rpmInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol Estane® 58246 Thermoplastic Polyurethane
Lubrizol ESTANE® 58133 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58149 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58130 Ester Based Thermoplastic Polyurethane
Lubrizol Estane® 58070 Thermoplastic Polyurethane

PNOVEON027 / 55293

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.