MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik Vestamid® Terra DS 18-GF-30 natural color 30% Glass Filled Nylon 1010  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: VESTAMID Terra DS18-GF30 is a 30% glass fiber-reinforced, easily demoldable and heat stabilized polyamide 1010 compound. Due to its mold release properties, VESTAMID Terra DS18-GF30 is suitable for the efficient production of injection molded parts with short cycle times. Products possess exceptional heat deflection temperature, a high durability and a good dimensional stability. VESTAMID Terra DS18-GF30 is supplied as cylindrical granules, ready for processing, in moisture-proof bags. VESTAMID® Terra DS is the polycondensation product of 1,10-decamethylene diamine (D) and 1,10-decanedioic acid (sebacic acid—S). Because both monomers are extracted from castor oil, VESTAMID® Terra DS is a material that is based 100% on natural resources.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.29 g/ccISO 1183
Water Absorption at Saturation 1.4 %ISO 62
Viscosity Number 180 cm³/gISO 307
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 136 MPaISO 527-1, ISO 527-2
Elongation at Break 5.0 %ISO 527-1, ISO 527-2
Elongation at Yield 4.0 %ISO 527-1, ISO 527-2
Tensile Modulus 7400 MPaISO 527-1, ISO 527-2
Charpy Impact Unnotched 95.0 kJ/m²
@Temperature 23.0 °C
complete break, incl. hinge break H; ISO 179-1/1 eU
 96.0 kJ/m²
@Temperature -30.0 °C
complete break, incl. hinge break H; ISO 179-1/1 eU
Charpy Impact, Notched 11.0 kJ/m²
@Temperature -30.0 °C
complete break, incl. hinge break H; ISO 179-1/1 eA
 19.0 kJ/m²
@Temperature 23.0 °C
complete break, incl. hinge break H; ISO 179-1/1 eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 206 °C2nd heating, DSC; ISO 11357
Vicat Softening Point 196 °C
@Load 5.10 kg
Method B; ISO 306
 201 °C
@Load 1.02 kg
Method A; ISO 306
 
Descriptive Properties
Global Warming Potential (kgCO2 equivalent/kg material)3.3Evonik, PE International, preliminary data
Renewable Carbon (%)100ASTM 6866

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cast Nylons Nycast® GF 30% Glass Filled Cast Nylon
EMS-Grivory Grilamid® 1SVX-50H nat PA1010-GF50
Domo TECHNYL® R AR 130/GF Nylon 66, 30% glass fiber, Conditioned
Suzhou Hipro Polymers Hiprolon® 70 MC HLS G30 Nylon 610, 30% glass fiber filled
EPICHEM Epinyl PA 66 GF 30 H Polyamide 66, 30% Glass, Heat Stabilized

PEVONIK988 / 192751

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.