MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Stratasys® Digital ABS  (discontinued **)
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; ABS Polymer

Material Notes: GREEN (RGD5160-DM, RGD5161-DM) MADE OF RGD515 & RGD535 |DIGITAL ABS, IVORY (RGD5130-DM, RGD5131-DM) MADE OF RGD515 & RGD531

Information provided by Stratasys

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.17 - 1.18 g/ccPolymerized; ASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 67 - 69
Hardness, Shore D 85 - 87
Tensile Strength at Break 55.0 - 60.0 MPaASTM D638-03
Elongation at Break 25 - 40 %ASTM D638-05
Modulus of Elasticity 2.60 - 3.00 GPaASTM D638-04
Flexural Strength 65.0 - 75.0 MPaASTM D790-03
Flexural Modulus 1700 - 2200 MPaASTM D790-04
Izod Impact, Notched 65.0 - 80.0 J/mASTM D256-06
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 58.0 - 68.0 °CASTM D648-06
 82.0 - 90.0 °Cafter thermal post treatment procedure A; ASTM D648-06
 92.0 - 95.0 °Cafter thermal post treatment procedure B; ASTM D648-06
Deflection Temperature at 1.8 MPa (264 psi) 51.0 - 55.0 °CASTM D648-07
Glass Transition Temp, Tg 47.0 - 53.0 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Markforged Onyx 3D Printed Nylon Carbon Composite
Markforged Kevlar® 3D Printed Composite
Markforged Carbon 3D Printed Composite
Lotte Advanced Materials Starex® SR-0300 Heat Resistant Grade ABS

PSTRAT245 / 206342

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.