MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Hifax CA 7442 A Thermoplastic Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Hifax polypropylene resins based on the Catalloy process are used in applications such as building and construction (e.g., single-ply roofing), industrial applications (e.g., wire and cable), and automotive industries. Hifax priovides good processability, excellent impact resistance, a broad range of stiffness from very soft to rigid products, high temperature resistance and low linear coefficient of thermal expansion.

Hifax CA 7442 A is a reactor TPO (thermoplastic polyolefin) manufactured using the LyondellBasell’s proprietary Catalloy process technology. It is primarily used for bumper and exterior trim applications in Automotive but can also be used as a base resin for technical compounds. It has a high impact performance and reduced shrinkage. The material also exhibits good processability. The grade is available in natural pellet form. Applications: Automotive Parts, Bumpers, Exterior Automotive Applications, Polymer Modifier.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0055 cm/cm0.0055 in/inInternal Method
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/inInternal Method
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
10 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 17.0 MPa2470 psi50mm/min; ISO 527-1,-2
Tensile Strength, Yield 19.0 MPa2760 psi50mm/min; ISO 527-1,-2
Flexural Modulus 1.00 GPa145 ksi2mm/min, chord; ISO 178
Charpy Impact, Notched  0.450 J/cm²
@Temperature -40.0 °C
2.14 ft-lb/in²
@Temperature -40.0 °F
Type 1, Edgewise, Notch A; ISO 179
 0.650 J/cm²
@Temperature -30.0 °C
3.09 ft-lb/in²
@Temperature -22.0 °F
Type 1, Edgewise, Notch A; ISO 179
 0.750 J/cm²
@Temperature -20.0 °C
3.57 ft-lb/in²
@Temperature -4.00 °F
Type 1, Edgewise, Notch A; ISO 179
 5.00 J/cm²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
Type 1, Edgewise, Notch A; ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 86.0 °C187 °Funannealed; ISO 75B-1,-2
Vicat Softening Point 121 °C250 °FB/50; ISO 306
 
Descriptive Properties
Processing MethodCompounding, Injection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQT7202 / 218839

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.