Insulating Aggregate raw material base. Hydraulic bond. A 1200°C insulating material with excellent strength, ideal for hot face insulation applications. Can be installed by casting, gunning or trowelling. Applications: General purpose insulating grade which can be used for hot face or back up insulation. Information provided by Morgan Advanced Materials |