MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Bayhydur® XP 2655 Polyurethane Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Polyurethane, TS

Material Notes: Hydrophilic aliphatic polyisocyanate based on hexamethylene diisocyanate (HDI). Hardener for waterborne two-component polyurethane systems.

Properties / Applications: Bayhydur® XP 2655 is a crosslinking agent for waterborne systems from which reliable incorporation and high chemical resistances are required. Despite its relatively low hydrophilia, this hardener can be easily dispersed in the aqueous phase, even at low shear forces such as are typically found in trade applications. Coatings formulated with the product yield films with high gloss and very low haze. The increase in viscosity during mixing that is typical for hydrophilized hardeners, in particular with ionically hydrophilized polyol dispersions, can be controlled by prethinning with water or slight amounts of organic cosolvent. The dispersibility of the product in water is influenced by organic cosolvents, but in different ways. The use of highly hydrophobic or highly hydrophilic cosolvents such as butyl acetate, xylene, butyl glycol acetate, dimethyl formamide or N-methylpyrrolidone generally leads to a coarser dispersion, which may cause turbidity in the coating film depending on the entire system. On the other hand, the use of, for example, methyl ethyl ketone, methoxypropyl acetate, dipropylene glycol dimethyl ether, propylene glycol diacetate or dicarboxylic acid diester mixtures leads to fine-particle dispersions. Because of the balance between moderate hydrophilization and high functionality, waterborne two-component polyurethane coatings formulated with Bayhydur® XP 2655 exhibit fast drying, rapid hardening with high ultimate hardness and excellent chemical resistance of the resultant films. Bayhydur® XP 2655 can also be used as the crosslinking partner for waterborne polyol binders (Bayhydrol®) and as a crosslinker for largely pH-neutral waterborne polymer dispersions such as polyurethane, polyvinyl acetate, polyacrylate and synthetic rubber dispersions. After addition of Bayhydur® XP 2655, the ready-to-use two-component formulation must be used within the pot life. This is not only governed by the polymer content but also by its other constituents (resin, thickener, plasticizer, etc.). With many dispersions, the end of this pot life – usually several hours – is not marked by gelling.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.16 g/cc1.16 g/ccDIN EN 2811
Viscosity 2500 - 4500 cP2500 - 4500 cPDIN EN ISO 3219/A.3
 
Thermal PropertiesMetricEnglishComments
Flash Point 192 °C378 °FDIN EN ISO 2719
 
Descriptive Properties
Color<60Hazen, M017-EN 1557
Content<0.24%Monomeric HDI, M106-ISO 10283
 10.3-21.3%NCO, M105-ISO 11909

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOVEST0202 / 201985

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.