SABIC LNP™ THERMOCOMP™ Compound PB006EQ Polyamide 6 (Nylon 6)
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
Material Notes:
LNP THERMOCOMP PB006EQ compound is based on Nylon 6 resin containing 30% glass bead. Added features of this grade include: Reduced Moisture.
Features: Low Moisture Absorption,Low Warpage,Structural
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.26
g/cc
0.0455
lb/in³
ISO 1183
Moisture Absorption
0.150 - 0.250 %
0.150 - 0.250 %
Injection Molding
Linear Mold Shrinkage, Flow
0.018
cm/cm
0.018
in/in
SABIC method
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
42.0
MPa
6090
psi
5 mm/min; ISO 527
Elongation at Break
10 %
10 %
5 mm/min; ISO 527
Flexural Strength
56.0
MPa
8120
psi
yield, 2 mm/min; ISO 178
Flexural Modulus
2.40
GPa
348
ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO)
4.00
kJ/m²
1.90
ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO)
40.0
kJ/m²
19.0
ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
109
µm/m-°C
@Temperature 23.0 - 60.0 °C
60.6
µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow
116
µm/m-°C
@Temperature 23.0 - 60.0 °C
64.4
µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi)
61.0
°C
142
°F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Processing Properties
Metric
English
Comments
Zone 2
255
-
265
°C
491
-
509
°F
Zone 3
265
-
275
°C
509
-
527
°F
Melt Temperature
255
-
275
°C
491
-
527
°F
Injection Molding
Mold Temperature
80.0
-
95.0
°C
176
-
203
°F
Drying Temperature
80.0
°C
176
°F
Injection Molding
Dry Time
4.00
hour
4.00
hour
Injection Molding
Back Pressure
0.300
-
0.700
MPa
43.5
-
102
psi
Screw Speed
30
-
60
rpm
30
-
60
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PSABH81764 / 289711
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.