System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Sharadaa Ceramics ZAP 011 Smart Cast Application
Categories:
Ceramic
Material Notes:
Special Properties: Thermal Shock, Accretion, Co, Impact Resistance
Industry: Sponge Iron
Application: Sponge Rotary Kiln
Information provided by Sharadaa Ceramics Pvt. Ltd.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Bulk Density
>=
2.40
g/cc
>=
0.0867
lb/in³
After Drying at 110°C
Grain Size
<=
10000
µm
<=
10000
µm
Mechanical Properties
Metric
English
Comments
Compressive Strength
68.6
MPa
@Temperature 110 °C
9960
psi
@Temperature 230 °F
Cold Crushing
88.3
MPa
@Temperature 1100 °C
12800
psi
@Temperature 2010 °F
Cold Crushing
118
MPa
@Temperature 1500 °C
17100
psi
@Temperature 2730 °F
Cold Crushing
29.4
MPa
@Time 86400 sec
4270
psi
@Time 24.0 hour
Cold Crushing
Thermal Properties
Metric
English
Comments
Maximum Service Temperature, Air
1500
°C
2730
°F
Descriptive Properties
Refractoriness
>1720°C
Thermal Expansion
0.5
@ 1000°C, Reversible
Water Required to Mix
5-5.5%
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
CSHARA135 / 130298
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.