MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Henkel Turco 5948-DPM Deoxidizer
Categories: Fluid; Solvent

Material Notes: Turco 5948-DPM is an alkaline, water-based, blue, concentrated compound formulated to effectively clean painted and unpainted aircraft exterior and interior surfaces when diluted with water. Ideally suited for use on all models of jet aircraft. It is also designed to be used in immersion tanks, for dip applications.
    Applications:
  • Metal Processing Lines
  • Jet Engine Cleaning
  • Aircraft Parts Cleaning
  • Aircraft Depaint & Repaint
  • Aircraft Appearance

Key Words: Aerospace Surface Treatment
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesOriginal ValueComments
Processing Temperature 65.0 - 80.0 °C
@Time 900 sec
 
Descriptive Properties
ChemistryAlkaline, Water-Based
ConsistencyLiquid
FormConcentrated
SubstrateAluminum
 Ferrous
 Magnesium
 Non-Ferrous
 Stainless Steel
 Titanium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Henkel Turco 5948-DPM Jet Cleaner, Exterior Wash
Henkel Turco Aldox V Deoxidizer
Henkel Turco T-4181L Liquid Alkaline Rust Remover
Henkel Turco Nitradd (T-4104) Deoxidizer
Henkel Turco Liquid Sprayeze NP-LT Deoxidizer

PHENK917 / 146922

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.