MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sandvik Iron Thermocouple
Categories: Metal; Ferrous Metal

Material Notes: Iron is the positive leg of thermocouples type J, L, and it is also the positive leg of compensating cables type KCA (WX). Thermocouple type J and L are frequently used because of their high emf output and their low cost. Compensating cables of type KCA are used together with thermocouples of type K.

IRON can not be exposed to sulphur containing atmospheres and to temperatures below zero. The alloy is transformed magnetically at 770°C, and a crystallographic transformation occurs at 900°C. Both transformations affect the thermoelectric properties of the alloy.

The wire is supplied copper-coated in order to prevent oxidation.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.86 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 100
@Thickness 2.00 mm
Tensile Strength, Ultimate 450 MPa
@Thickness 2.00 mm
Elongation at Break 15 %
@Thickness 2.00 mm
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000130 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.7 µm/m-°C
@Temperature 20.0 - 100 °C
Specific Heat Capacity 0.445 J/g-°C
@Temperature 20.0 °C
Thermal Conductivity 66.2 W/m-K
@Temperature 100 °C
Melting Point 1535 °C
Maximum Service Temperature, Air 560 °C
@Thickness 0.250 mm
bare
 650 °C
@Thickness 0.500 mm
bare
 670 °C
@Thickness 0.250 mm
protected
 720 °C
@Thickness 1.00 mm
bare
 760 °C
@Thickness 1.00 mm
protected
 760 °C
@Thickness 3.26 mm
bare
 760 °C
@Thickness 3.26 mm
protected
 760 °C
@Thickness 1.63 mm
bare
 760 °C
@Thickness 1.63 mm
protected
 760 °C
@Thickness 0.500 mm
protected
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.030 %
Iron, Fe 99.62 %
Manganese, Mn 0.30 %
Silicon, Si 0.050 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Thermal Ceramics TE 1800 Board and Shapes Molded Min-K Insulation
Thermal Ceramics TE 1400 Board and Shapes Molded Min-K Insulation
Thermal Ceramics TE 1200 Board and Shapes Molded Min-K Insulation
Thermal Ceramics 1302 Board and Shapes Molded Min-K Insulation
Sandvik Nisil Thermocouple Alloy

NSANDV105 / 18999

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.