MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Ryton® QC160N PPS, High viscosity for stock shapes and film
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: High viscosity PPS polymer for stock shapes and film

Ryton® QC160N (granular powder) unfilled polyphenylene sulfide exhibits excellent thermal stability and chemical resistance and is suitable for thermoplastic extrusion processes.

Markets/Uses: Films / High Temperature Films / Thin Films and Tapes

Applications: Film; Stock Material for Machining

Features: Chemical Resistant; Good Thermal Stability

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.34 g/ccASTM D792
Volatiles <= 0.30 %
@Temperature 150 °C
Water Absorption 0.050 %
@Time 86400 sec
ASTM D570
Melt Flow 45 g/10 minProcedure B; ASTM D1238
Ash 0.30 %ISO 3451-1
 
Mechanical PropertiesOriginal ValueComments
Tensile Stress 75.0 MPaISO 527-2
Elongation at Break 6.0 %ISO 527-2
Tensile Modulus 3400 MPaISO 527-2
Flexural Strength 130 MPaISO 178
Flexural Modulus 3400 MPaISO 178
Izod Impact, Notched 53.0 J/m
@Thickness 3.18 mm
ASTM D256
Izod Impact, Notched (ISO) 4.00 kJ/m²Notch A; ISO 180
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Surface Resistance 1.00e+16 ohmASTM D257
Dielectric Constant 3.2
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 24.0 kV/mmASTM D149
Dissipation Factor 0.0020
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 50.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
ASTM E831
 120 µm/m-°C
@Temperature 100 - 200 °C
ASTM E831
Thermal Conductivity 0.300 W/m-KASTM C177
Melting Point 280 °CISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 160 °CUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °CUnannealed; ASTM D648
Vicat Softening Point >= 180 °CISO 306
Glass Transition Temp, Tg 90.0 °CISO 11357-2
Flammability, UL94 V-0
@Thickness 1.60 mm
Oxygen Index 44 %ASTM D2863
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorNatural Color
FormsPowder
ProcessingExtrusion
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4414 / 280214

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.