MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Shin-Etsu Silicones KE-941U Silicone Elastomer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber

Material Notes: KE941 U is one of a series of easy processing, general purpose silicone rubber bases. It can be used in a variety of applications requiring finishing by molding (compression, injection, transfer).

Product Features:

  • Rubber contacts.
  • Food packing.
  • Industrial packing.
  • Diaphragms.

Information Provided by Shin-Etsu Silicones of America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40
Tensile Strength at Break 1065 psi
Elongation at Break 385 %
Tear Strength 56.0 pliDie B
Compression Set 10 %
@Temperature 149 °C,
Time 79200 sec
 
Processing PropertiesOriginal ValueComments
Cure Time 4.00 hour
@Temperature 200 °C
Post
 
Descriptive Properties
Cure AgentDBPH
Cure TypePost Cure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Shin-Etsu Silicones KE-951U Silicone Elastomer
Magnesium AZ91D-F, Cast
Aluminum 384.0-F Die Casting Alloy
Shin-Etsu Silicones KE-347T Silicone, RTV Coating
Shin-Etsu Silicones KE-441 Silicone, RTV

PSHIN237 / 177748

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.