MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® A 60 G2 V30 PA66, 30% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Description: High flow Polyamide PA66 Flame retarded grade reinforced with 30% glass fiber, for injection molding.

Available in: Asia Pacific, Europe, Latin America and North America

Product Applications: This Red Phosphorous and Halogen free flame retardant grade, combines excellent all-round mechanical properties with outstanding flame retardancy. This product is ideally suited for large and small appliances and connectic applications requiring glow wire no flame performance. This product is registered at the VDE institute for the IEC 60335 normative in all color references down to 0.8mm thickness. It has a robust GWIT/GWT pass with excellent CTI (>550V) and ball pressure test performance (>150°C). This product is available in Natural, Grey and Black. Specific colors and Laser Marking grades optimized for YAG and UV laser types are also available upon request.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.46 g/ccISO 1183/A
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 150 MPaISO 527 Type 1A
Elongation at Break 2.5 %ISO 527 Type 1A
Tensile Modulus 11500 MPaISO 527 Type 1A
Charpy Impact Unnotched 55.0 kJ/m²ISO 179/1eU
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 600 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 262 °CISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 256 °CISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 247 °CISO 75/Af
Flammability, UL94 V-0
@Thickness 0.800 mm
1210
 V-0
@Thickness 1.60 mm
1210
 V-0
@Thickness 3.20 mm
1210
Glow Wire Ignition Temperature 800 °C
@Thickness 0.800 mm
ISO 60695-2-13
 850 °C
@Thickness 1.60 mm
ISO 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 0.800 mm
ISO 60695-2-12
 960 °C
@Thickness 1.60 mm
ISO 60695-2-12
 960 °C
@Thickness 3.20 mm
ISO 60695-2-12
 
Processing PropertiesOriginal ValueComments
Feed Temperature 265 - 275 °C
Mold Temperature 60.0 - 90.0 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone265-275°C
Mixing Zone270-280°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® A 60 G1 V25 PA66, 25% glass fiber, DRY
Domo TECHNYL® A 60 G1 V30 PA66, 30% glass fiber, DRY
Domo TECHNYL® A 60 G2 V30 PA66, 30% glass fiber, Conditioned
Domo Technyl® A 60G1 V25 25% Glass Reinforced Nylon 66, Flame Retardant
Domo Technyl® A20V25 25% Glass Filled, V-0 Nylon 66

PRHOD726 / 137957

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.