MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Telcar® TELC-87-L832-A Thermoplastic Elastomer
Categories: Polymer; Thermoplastic

Material Notes: Telcar TELC-87-L832-A is a general purpose thermoplastic elastomer designed for wire & cable applications requiring flexibility over a wide temperature range. It is a low density, medium hardness, low halogen content, UV stabilized grade that has good impact resistance and is suitable for extrusion.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Good Impact Resistance; Low Density; Low Halogen Content; UV Resistant

Uses: General Purpose; Wire & Cable Applications

RoHS Compliant:RoHS Compliant

Form: Pellets

Processing Method: Extrusion; Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.885 g/cc0.0320 lb/in³ASTM D792
Viscosity 639 cP
@Shear Rate 206 1/s,
Temperature 200 °C
639 cP
@Shear Rate 206 1/s,
Temperature 392 °F
ASTM D3835
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 75
@Time 5.00 sec
75
@Time 0.00139 hour
ISO 868
 76.5
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
76.5
@Treatment Temp. 230 °F,
Time 1008 hour
Change in Air; ISO 888
Tensile Strength at Break 5.80 MPa841 psiAcross Flow; ASTM D412
 5.80 MPa841 psiFlow; ASTM D412
 6.15 MPa
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
892 psi
@Treatment Temp. 230 °F,
Time 1008 hour
Across Flow, Change in Air; ISO 188
 6.18 MPa
@Treatment Temp. 125 °C,
Time 605000 sec
896 psi
@Treatment Temp. 257 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
Tensile Strength  2.79 MPa
@Treatment Temp. 125 °C,
Time 605000 sec
405 psi
@Treatment Temp. 257 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
 3.20 MPa
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
464 psi
@Treatment Temp. 230 °F,
Time 1008 hour
Across Flow, Change in Air; ISO 188
Tensile Stress at Strain  2.76 MPa
@Strain 100 %
400 psi
@Strain 100 %
Across Flow; ASTM D412
 3.83 MPa
@Strain 100 %
555 psi
@Strain 100 %
Flow; ASTM D412
Elongation at Break 320 %320 %Flow; ASTM D412
 540 %540 %Across Flow; ASTM D412
Tear Strength 37.0 kN/m211 pliAcross Flow; ASTM D624
Compression Set  28 %
@Temperature 22.8 °C,
Time 79200 sec
28 %
@Temperature 73.0 °F,
Time 22.0 hour
ASTM D695
 58 %
@Temperature 70.0 °C,
Time 79200 sec
58 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D695
 68 %
@Temperature 90.0 °C,
Time 252000 sec
68 %
@Temperature 194 °F,
Time 70.0 hour
ASTM D695
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.24
@Frequency 1000 Hz
2.24
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -60.0 °C<= -76.0 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Zone 1 166 - 188 °C330 - 370 °FExtrusion
Zone 2 171 - 193 °C340 - 380 °FExtrusion
Zone 3 177 - 199 °C350 - 390 °FExtrusion
Zone 5 182 - 204 °C360 - 400 °FExtrusion
Die Temperature 190 - 210 °C374 - 410 °FExtrusion
Screw Speed 30 - 100 rpm30 - 100 rpmExtrusion
 
Descriptive Properties
AppearanceClear/Transparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ1627 / 238118

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.