MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ATI Allegheny Ludlum AL 412™ Dual Phase 12% Cr
Categories: Metal; Ferrous Metal; Stainless Steel; T S40000 Series Stainless Steel

Material Notes: Low carbon, nickel containing, dual phase 12% Cr stainless steel alloy.

Characteristics: superior toughness to ferritic alloys, high strength, high corrosion resistance.

Information provided by Allegheny Ludlum

Key Words: UNS S41003
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 87
Tensile Strength, Ultimate 565 MPa
Tensile Strength, Yield 414 MPa
@Strain 0.2 %
Elongation at Break 24 %in 2"
Charpy Impact 50.0 ft-lb
@Temperature -73.3 °C
Transverse
 85.0 ft-lb
@Temperature -73.3 °C
Longitudinal
 280 ft-lb
@Temperature 15.6 °C
Longitudinal
 280 ft-lb
@Temperature 15.6 °C
Transverse
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.020 %
Chromium, Cr 11.75 %
Iron, Fe >= 86.13 %As Remainder
Manganese, Mn 0.90 %
Nickel, Ni 0.40 %
Nitrogen, N <= 0.030 %
Phosphorus, P <= 0.040 %
Silicon, Si 0.70 %
Sulfur, S <= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
American Utility Metals Cromgard® Stainless Steel
Ametek Ultra 303L P/M Stainless Steel, Sintered from 6.0 g/cc Green Density
ArcelorMittal Dual Phase 780 Very High Strength Hot Rolled Steel
ArcelorMittal Dual Phase 980 LCE Y600 Very High Strength Cold Rolled Steel
Ametek Ultra 304L P/M Stainless Steel, Sintered from 6.75 g/cc Green Density

NL1018 / 17786

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.