MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Akulon® K240-HP Impact Modified Nylon 6 (European Grade) (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier film, stock shapes, convoluted tubes, and monofilament. Akulon XP is a high-productivity, high-performance PA6 grade for film extrusion processes. Medium viscosity, unreinforced or reinforced Akulon grades are used for various injection molding and blow molding applications. Akulon® Ultraflow® is a high-productivity, high-performance PA6 family for molding processes.

Key applications for Akulon:

  • Automotive: Intake manifold, Engine, Powertrain, Airbag containers, Exterior trim, Interior trim, Electrical components and connectors
  • Consumer durables: Power tools, Lawn and garden tools, Small appliances, Sports and leisure equipment, Furniture, Industrial Goods, Transportation
  • E&E: Low voltage switch gear/power distribution, Lighting, Power connectors
  • Film: Specialty and barrier films

Information provided by DSM.

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/ccISO 1183
Water Absorption 9.0 %Sim. to ISO 62
Moisture Absorption at Equilibrium 3.0 %Humidity Absorption; Sim. to ISO 62
High Load Melt Index 44 g/10 min
@Load 21.6 kg,
Temperature 275 °C
Calculated from Volume Flow Rate of 40 cm3/10min.; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 60.0 MPaISO 527-1/-2
Elongation at Break >= 50 %ISO 527-1/-2
Elongation at Yield 4.0 %ISO 527-1/-2
Tensile Modulus 2.70 GPaISO 527-1/-2
Charpy Impact Unnotched NB
@Temperature -30.0 °C
ISO 179/1eU
 NB
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 2.00 J/cm²
@Temperature -30.0 °C
ISO 179/1eA
 5.00 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 100 µm/m-°C
@Temperature 20.0 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 140 µm/m-°C
@Temperature 20.0 °C
ISO 11359-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 170 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °CISO 75-1/-2
Flammability, UL94 HB
@Thickness 1.60 mm
IEC 60695-11-10
 
Descriptive Properties
Blow MoldingYes
Heat Stabilized or Stable to HeatYes
High Impact or Impact ModifiedYes
Without FillersYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zytel® BM70G20HSLX BK537 PA66-IGF20

PDSMEU186 / 31214

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.