MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Saint-Gobain Furon® C950 DuraForm™ C950 Thermal Phase Change Microprocessor Interface Material
Categories: Polymer; Adhesive

Material Notes: Description: A 4.5 mil thick thermally conductive, adhesive-based material which changes phase at 53°C to assure maximum surface conformance. Recommended uses include high-performance microprocessors and applications with surface roughness and/or concavity problems. Application advantages: Minimizes system assembly cost by allowing for pre-attachment to the heat sink or CPU; Softens and conforms to surface roughness or concavity at operating temperature; Operates at low clip pressures (5 to 10 psi); Applies and repositions with thumb pressure for easy field service; Allows for vertical mounting due to cohesive properties. All data based on a 0.0045 inch test sample.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.23e+13 ohm-cmASTM D1000
Dielectric Strength 650 V/milASTM D1000
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.640 W/m-KSample area of 1 square inch at 10 psi.; ASTM E1530
Melting Point 127.4 °FASTM E1530
 
Descriptive Properties
ColorBlue
Thermal Resistance0.08°C/WASTM E1530

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tra-Con Tra-Pad PCAA8A Thermally Conductive Phase Change Material
Honeywell PTM3180 Phase Change Thermal Interface Material

PSTGQZ476 / 68990

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.