MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Master Bond EP46HT-1ND2 Two Component Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Epoxy, High Temperature

Material Notes: Key Features:
  • Glass transition temperature over 240°C
  • Impressive chemical resistance
  • Outstanding electrical insulation properties
  • Long pot life at room temperature
  • Service temperature range of -100°F to +600°F
  • High bonding strength
Product Description: Master Bond EP46HT-1ND2 is a two part epoxy system for high performance structural bonding and sealing, suitable for applications where resistance to temperatures from -100°F to +600°F is required. It is 100% reactive and does not contain any solvents or diluents. While it does not cure at room temperature, it does cure readily at elevated temperatures. A good curing schedule to optimize properties is 2 hours at 300°F, followed by a few hours at 350-400°F. The cured epoxy produces bonds and seals with high mechanical strength and excellent chemical resistance. EP46HT-1ND2 has a forgiving 100 to 30 mix ratio by weight. It should be noted that EP46HT-1ND2 is relatively exothermic and should not be cured in sections greater than 10-20 thousandths of an inch thick and a bondline thickness is typically 2-6 thousandths of an inch. EP46HT-1ND2 has a paste consistency and will not flow when applied or during curing. EP46HT-1ND2 can withstand intense thermal cycling and resist many chemicals, including water, oils, solvents, bases and acids. It bonds exceptionally well to metals, composites, glass, ceramics and many plastics. Once cured, the system is a top flight electrical insulator. The color of Part A is tan and Part B is moderately dark brown. EP46HT-1ND2 is normally used in demanding applications found in the aerospace, electronic and specialty OEM industries where exceptional thermal and chemical resistance along with the non-drip application feature might be required.

Product Advantages:

  • Easy application, smooth paste viscosity
  • Convenient cure schedules at elevated temperatures
  • Outstanding heat resistance and thermal stability
  • Robust chemical resistance
  • First rate electrical insulation properties even upon prolonged exposure to hostile environments
  • Working life over 24 hours at room temperature
  • Won’t “run” when applied or during curing

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 80 - 9080 - 90
Tensile Strength >= 75.8 MPa>= 11000 psi
Elongation at Break 2.0 - 5.0 %2.0 - 5.0 %
Tensile Modulus 3.10 - 3.45 GPa450 - 500 ksi
Compressive Strength >= 124 MPa>= 18000 psi
Adhesive Bond Strength >= 15.2 MPa>= 2200 psiTensile lap, Aluminum to Aluminum
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cm
Dielectric Strength 17.7 kV/mm
@Thickness 3.17 mm
450 kV/in
@Thickness 0.125 in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 30.0 - 35.0 µm/m-°C16.7 - 19.4 µin/in-°F
Maximum Service Temperature, Air 316 °C600 °F
Minimum Service Temperature, Air -73.3 °C-100 °F
Glass Transition Temp, Tg >= 240 °C>= 464 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 120 min2.00 hourPost cure for optimum properties at 350-400°F
 120 - 180 min
@Temperature 121 - 149 °C
2.00 - 3.00 hour
@Temperature 250 - 300 °F
Working Life >= 1440 min>= 1440 minAfter mixing, 100 g batch
Shelf Life 12.0 Month
@Temperature <=23.9 °C
12.0 Month
@Temperature <=75.0 °F
in original, unopened containers
 
Descriptive Properties
Mixing Ratio100:30 by weightParts A to B
Viscositysmooth pasteMixed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond EP113 Two Component Epoxy
Master Bond EP121AO Thermally Conductive, Dimensionally Stable Epoxy System
Master Bond Supreme 42HT-2ND-2 Two Component Epoxy
Master Bond Supreme 42HT-2ND Two Component Epoxy
Master Bond Supreme 12AOHT-LO One Component Epoxy

PMASTM885 / 185478

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.