Description: AKROMID B3 2 RM-D black (3255) is a nonreinforced, UV-stabilized polyamide 6 with limited moisture absorption. Applications are interior and exterior parts with improved impact strength in the automotive industry. Additive: UV Stabilizer Features: - Good Impact Resistance
- Low Moisture Absorption
Uses:- Automotive Applications
- Automotive Exterior Parts
- Automotive Interior Parts
Information provided by Akro-Plastic GmbH |