MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ MC5 Metal Instant Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: 3M™ Scotch-Weld™ Metal Instant Adhesives are designed to give optimum performance and high strength bonds on metals, including galvanized or anodized surfaces. MC5 (formerly SP93) is a very low viscosity cyanoacrylate primarily used for bonding smooth, even, close fitting parts. It is a wicking type cyanoacrylate that can be used in preassembled parts. It has been tested and passed the requirements of Commercial Item Description A-A-3097, Type 1, Class 1 (formerly MIL-A-46050C).

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.09 g/cc
Viscosity 2.0 - 5.0 cPU-Tube IC-C45
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 3100 psiOverlap, grit-blasted steel; ASTM D1002
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 82.0 °C
Minimum Service Temperature, Air -54.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 0.250 - 0.583 minTime to Handling Strength
 24.0 hourFull Cure
 
Descriptive Properties
AppearanceClear Liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Special Metals INCOLOY® Alloy 825
Outokumpu 2205 Duplex Stainless Steel
Industeel URANUS® 45N 22Cr 3Mo Duplex Stainless Steel with PREN = 33 or 34
Carlson 2205 (UNS S31803) Duplex Stainless Steel
316 Stainless Steel, annealed sheet

PMM34722 / 169469

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.