MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Polyetherimide (PEI)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Ensinger TECAPEI™ shapes combine Ultem® PEI polymer with Ensinger's proprietary extrusion techniques for exceptional reliability, consistency, dimensional stability, and high temperature mechanical performance. FDA, USP Class VI and NSF compliant.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.0500 - 1.90 g/ccAverage value: 1.38 g/cc Grade Count:665
Filler Content 5.00 - 50.0 %Average value: 30.2 % Grade Count:67
Water Absorption 0.0150 - 1.30 %Average value: 0.225 % Grade Count:222
Moisture Absorption at Equilibrium 0.000 - 1.30 %Average value: 0.198 % Grade Count:370
Water Absorption at Saturation 0.100 - 2.90 %Average value: 1.06 % Grade Count:220
Additive Loading 10.0 - 40.0 %Average value: 20.2 % Grade Count:32
Particle Size 15.0 µmAverage value: 15.0 µm Grade Count:3
Viscosity 3.00 - 87.0 cP
@Temperature 220 - 360 °C
Average value: 16.8 cP Grade Count:161
 3.00 - 87.0 cP
@Load 2.16 - 10.0 kg
Average value: 16.8 cP Grade Count:161
Maximum Moisture Content 0.0200Average value: 0.0200 Grade Count:3
Linear Mold Shrinkage 0.000 - 0.0230 cm/cmAverage value: 0.00440 cm/cm Grade Count:519
Linear Mold Shrinkage, Transverse 0.00100 - 0.0240 cm/cmAverage value: 0.00535 cm/cm Grade Count:160
Melt Flow 1.80 - 113 g/10 minAverage value: 13.8 g/10 min Grade Count:271
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 85.0 - 115Average value: 110 Grade Count:95
Hardness, Rockwell R 100 - 127Average value: 119 Grade Count:48
Hardness, Shore D 72.0 - 93.0Average value: 84.4 Grade Count:17
Ball Indentation Hardness 125 - 220 MPaAverage value: 149 MPa Grade Count:90
Tensile Strength, Ultimate 1.00 - 650 MPaAverage value: 134 MPa Grade Count:548
Tensile Strength, Yield 20.0 - 255 MPaAverage value: 114 MPa Grade Count:305
Elongation at Break 0.500 - 110 %Average value: 21.4 % Grade Count:622
Elongation at Yield 0.700 - 400 %Average value: 8.05 % Grade Count:191
Modulus of Elasticity 0.00280 - 56.0 GPaAverage value: 7.75 GPa Grade Count:574
Flexural Yield Strength 17.9 - 770 MPaAverage value: 192 MPa Grade Count:624
 85.0 - 214 MPa
@Temperature 80.0 - 200 °C
Average value: 151 MPa Grade Count:2
Flexural Modulus 0.380 - 46.0 GPaAverage value: 7.23 GPa Grade Count:632
 7.30 - 17.9 GPa
@Temperature 80.0 - 200 °C
Average value: 12.4 GPa Grade Count:2
Flexural Strain at Break 0.900 - 3.80 %Average value: 2.45 % Grade Count:12
 1.00 - 2.60 %
@Temperature 80.0 - 200 °C
Average value: 1.89 % Grade Count:2
Compressive Yield Strength 0.500 - 1130 MPaAverage value: 230 MPa Grade Count:60
Compressive Modulus 0.0220 - 52.0 GPaAverage value: 13.0 GPa Grade Count:33
Poissons Ratio 0.300 - 0.440Average value: 0.368 Grade Count:33
Shear Modulus 0.0130 - 4.73 GPaAverage value: 2.33 GPa Grade Count:10
Shear Strength 0.600 - 128 MPaAverage value: 77.4 MPa Grade Count:21
Izod Impact 16.0 - 3300 JAverage value: 452 J Grade Count:275
 20.0 - 120 J
@Temperature -30.0 - -30.0 °C
Average value: 54.1 J Grade Count:57
Izod Impact, Notched 0.0298 - 19.2 J/cmAverage value: 1.10 J/cm Grade Count:260
 0.350 - 0.742121 J/cm
@Temperature -30.0 - -30.0 °C
Average value: 0.460 J/cm Grade Count:11
Izod Impact, Unnotched 0.120 J/cm - NBAverage value: 7.43 J/cm Grade Count:343
 15.0 - 99.99 J/cm
@Temperature -30.0 - -30.0 °C
Average value: 15.2 J/cm Grade Count:23
Izod Impact, Notched (ISO) 2.00 kJ/m² - NBAverage value: 7.95 kJ/m² Grade Count:202
 2.00 kJ/m² - NB
@Temperature -40.0 - -30.0 °C
Average value: 7.89 kJ/m² Grade Count:127
 5.00 - 5.00 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 7.89 kJ/m² Grade Count:1
 5.00 - 5.00 kJ/m²
@Thickness 4.00 - 4.00 mm
Average value: 7.89 kJ/m² Grade Count:1
Izod Impact, Unnotched (ISO) 5.00 kJ/m² - NBAverage value: 33.4 kJ/m² Grade Count:175
 13.0 kJ/m² - NB
@Temperature -40.0 - -30.0 °C
Average value: 32.2 kJ/m² Grade Count:112
 NB - NB
@Temperature -30.0 - -30.0 °C
Average value: 32.2 kJ/m² Grade Count:1
 NB - NB
@Thickness 3.00 - 3.00 mm
Average value: 32.2 kJ/m² Grade Count:1
Charpy Impact Unnotched 0.0110 J/cm² - NBAverage value: 3.54 J/cm² Grade Count:67
 1.40 J/cm² - NB
@Temperature -30.0 - -30.0 °C
Average value: 3.44 J/cm² Grade Count:51
Charpy Impact, Notched 0.200 J/cm² - NBAverage value: 0.777 J/cm² Grade Count:154
 0.300 - 1.00 J/cm²
@Temperature -30.0 - -30.0 °C
Average value: 0.523 J/cm² Grade Count:57
Gardner Impact 2.26 - 36.0 JAverage value: 29.5 J Grade Count:56
Dart Drop, Total Energy 2.00 - 380 JAverage value: 27.9 J Grade Count:108
 88.0 - 99.0 J
@Temperature -20.0 - 0.000 °C
Average value: 94.8 J Grade Count:6
Falling Dart Impact 4.90 - 21.4 JAverage value: 9.18 J Grade Count:17
Instrumented Impact Total Energy 1.48 - 38.0 JAverage value: 20.1 J Grade Count:19
Coefficient of Friction 0.110 - 0.770Average value: 0.387 Grade Count:40
Coefficient of Friction, Static 0.110 - 0.630Average value: 0.405 Grade Count:31
Tear Strength 37.0 - 147 kN/mAverage value: 73.7 kN/m Grade Count:3
K Factor (Wear Factor) 27.0 - 1900Average value: 605 Grade Count:5
K (wear) Factor 40.3 - 423 x 10-8 mm³/N-MAverage value: 147 x 10-8 mm³/N-M Grade Count:28
Limiting Pressure Velocity 1.90 - 2.10 MPa-m/secAverage value: 2.00 MPa-m/sec Grade Count:6
Taber Abrasion, mg/1000 Cycles 2.00 - 60.0Average value: 16.4 Grade Count:93
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0500 - 1.00e+18 ohm-cmAverage value: 2.59e+16 ohm-cm Grade Count:303
Surface Resistance 1.00 - 5.80e+16 ohmAverage value: 1.38e+15 ohm Grade Count:219
Static Decay 0.0100 - 2.00 secAverage value: 1.10 sec Grade Count:46
Shielding Effectiveness 50.0 - 97.0 dBAverage value: 78.6 dB Grade Count:3
Dielectric Constant 2.52 - 6.80Average value: 3.18 Grade Count:182
Dielectric Strength 4.33 - 244 kV/mmAverage value: 25.7 kV/mm Grade Count:181
Dissipation Factor 0.000500 - 0.266Average value: 0.00357 Grade Count:173
Dielectric Loss Index 0.00100 - 0.00150Average value: 0.00133 Grade Count:4
Arc Resistance 0.000 - 180 secAverage value: 118 sec Grade Count:166
Comparative Tracking Index 0.000 - 250 VAverage value: 133 V Grade Count:217
Hot Wire Ignition, HWI 7.00 - 120 secAverage value: 66.9 sec Grade Count:185
High Amp Arc Ignition, HAI 0.000 - 120 arcsAverage value: 21.7 arcs Grade Count:184
High Voltage Arc-Tracking Rate, HVTR 0.000 - 150 mm/minAverage value: 86.5 mm/min Grade Count:162
 
Thermal PropertiesOriginal ValueComments
CTE, linear 2.70 - 120 µm/m-°CAverage value: 36.4 µm/m-°C Grade Count:378
 5.00 - 60.0 µm/m-°C
@Temperature 40.0 - 205 °C
Average value: 34.3 µm/m-°C Grade Count:8
CTE, linear, Transverse to Flow 5.00 - 130 µm/m-°CAverage value: 49.3 µm/m-°C Grade Count:262
 62.5 - 62.5 µm/m-°C
@Temperature 40.0 - 120 °C
Average value: 62.5 µm/m-°C Grade Count:1
Specific Heat Capacity 1.10 - 6.28 J/g-°CAverage value: 3.00 J/g-°C Grade Count:6
Thermal Conductivity 0.0360 - 11.0 W/m-KAverage value: 0.321 W/m-K Grade Count:176
Melting Point 171 - 254 °CAverage value: 222 °C Grade Count:10
Maximum Service Temperature, Air 70.0 - 300 °CAverage value: 181 °C Grade Count:51
Hot Ball Pressure Test 75.0 - 125 °CAverage value: 125 °C Grade Count:105
Transformation Temperature, Tg 168 - 200 °CAverage value: 192 °C Grade Count:5
Deflection Temperature at 0.46 MPa (66 psi) 116 - 237 °CAverage value: 208 °C Grade Count:310
Deflection Temperature at 1.8 MPa (264 psi) 47.2 - 393 °CAverage value: 200 °C Grade Count:587
Vicat Softening Point 75.0 - 242 °CAverage value: 214 °C Grade Count:242
Minimum Service Temperature, Air -50.0 - 0.000 °CAverage value: -30.0 °C Grade Count:11
Glass Transition Temp, Tg 180 - 220 °CAverage value: 212 °C Grade Count:50
UL RTI, Electrical 105 - 180 °CAverage value: 145 °C Grade Count:225
UL RTI, Mechanical with Impact 105 - 180 °CAverage value: 143 °C Grade Count:228
UL RTI, Mechanical without Impact 105 - 180 °CAverage value: 145 °C Grade Count:228
Flammability, UL94 HB - 5VAGrade Count:375
Smoke Density 0.000 - 10.0Average value: 2.63 Grade Count:56
Oxygen Index 44.0 - 54.0 %Average value: 47.3 % Grade Count:127
Glow Wire Test 825 - 960 °CAverage value: 930 °C Grade Count:73
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 58.0 - 90.0 %Average value: 84.3 % Grade Count:6
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 410 °CAverage value: 295 °C Grade Count:69
Nozzle Temperature 173 - 421 °CAverage value: 374 °C Grade Count:356
Adapter Temperature 270 - 335 °CAverage value: 303 °C Grade Count:7
Die Temperature 260 - 360 °CAverage value: 327 °C Grade Count:26
Melt Temperature 107 - 427 °CAverage value: 312 °C Grade Count:483
Head Temperature 290 - 360 °CAverage value: 341 °C Grade Count:19
Mold Temperature 37.8 - 399 °CAverage value: 151 °C Grade Count:510
Drying Temperature 60.0 - 152 °CAverage value: 146 °C Grade Count:491
Moisture Content 0.0200 - 0.0400 %Average value: 0.0332 % Grade Count:110
Dew Point -28.9 °CAverage value: -28.9 °C Grade Count:70
Injection Pressure 82.7 - 124 MPaAverage value: 103 MPa Grade Count:111
Vent Depth 0.00250 - 0.00760 cmAverage value: 0.00500 cm Grade Count:275
Precipitation Temperature 60.0 - 120 °CAverage value: 95.6 °C Grade Count:65

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyetheretherketone, Unreinforced
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
Overview of materials for Polysulfone (PSU)
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Overview of materials for Polyetherketoneketone (PEKK), Unreinforced

O3600 / 77777

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.