System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Kolon ELLAS K-395A Ether Based Thermoplastic Polyurethane
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Elastomer, TPE
;
Polyurethane, TP
;
Thermoplastic Polyurethane, Elastomer, Ether Grade
Material Notes:
Applications
Extrusion
Injection: Cable sheathing, Highly Pressurized Hose
Industry Parts
Information provided by API-Kolon.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.12
g/cc
ASTM D792
Mechanical Properties
Original Value
Comments
Hardness, Shore A
95
ASTM D2240
Tensile Strength
460
kg(f)/cm²
ASTM D412
Tensile Stress at Strain
120
kg(f)/cm²
@Strain 100 %
ASTM D412
Elongation at Break
500 %
ASTM D412
Tear Strength
140
kg(f)/cm
ASTM D624
Processing Properties
Original Value
Comments
Nozzle Temperature
185
-
195
°C
Injection Molding
Zone 1
160
-
175
°C
Injection Molding
160
-
175
°C
Extrusion Molding
Zone 2
170
-
185
°C
Extrusion Molding
175
-
185
°C
Injection Molding
Zone 3
170
-
190
°C
Extrusion Molding
180
-
190
°C
Injection Molding
Zone 4
180
-
195
°C
Extrusion Molding
Die Temperature
180
-
195
°C
Extrusion Molding
Head Temperature
190
-
200
°C
Extrusion Molding
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Ravago Petrochemical Ravathane® R210A93UV Ether-Based Thermoplastic Polyurethane
Covestro Platilon® 4201 AU Polyurethane (Ether) Film
Clariant Renol PURSP0002 Polyurethane Elastomer, Ether Based
Huntsman IROGRAN® A 85 P 4441 FCM Ether-Based TPU-For Food Contact
Dow Pellethane® 2351-85AE Polyurethane Elastomer, Ether Based
PKOKZ985 / 122687
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.