System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Star Plastics ReStart™ ABS6000 Molding Grade ABS, 50% Recycled
Categories:
Polymer
;
Renewable/Recycled Polymer
;
Thermoplastic
;
ABS Polymer
;
Acrylonitrile Butadiene Styrene (ABS), Molded
Material Notes:
Molding Grade General Purpose ABS, including 50% Certified Recycled Content Materials. Furnished as Pellets. May be used to produce molded or extruded articles or as a component of other industrial products.
Information provided by Star Plastics.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.05
g/cc
1.05
g/cc
ASTM D792
Linear Mold Shrinkage
0.0050
-
0.0080
cm/cm
0.0050
-
0.0080
in/in
ASTM D955
Melt Flow
5.0
g/10 min
@Load 3.80 kg,
Temperature 230 °C
5.0
g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
40.0
MPa
5800
psi
ASTM D638
Tensile Modulus
2.00
GPa
290
ksi
ASTM D638
Flexural Yield Strength
58.6
MPa
8500
psi
ASTM D790
Flexural Modulus
2.07
GPa
300
ksi
ASTM D790
Izod Impact, Notched
1.87
J/cm
@Thickness 3.17 mm,
Temperature 22.8 °C
3.50
ft-lb/in
@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
76.7
°C
@Thickness 3.17 mm
170
°F
@Thickness 0.125 in
ASTM D648
Processing Properties
Metric
English
Comments
Rear Barrel Temperature
188
-
218
°C
370
-
425
°F
Middle Barrel Temperature
204
-
232
°C
400
-
450
°F
Front Barrel Temperature
218
-
246
°C
425
-
475
°F
Nozzle Temperature
218
-
274
°C
425
-
525
°F
Melt Temperature
218
-
274
°C
425
-
525
°F
Mold Temperature
48.9
-
76.7
°C
120
-
170
°F
Drying Temperature
82.2
-
93.3
°C
@Time 7200 - 14400 sec
180
-
200
°F
@Time 2.00 - 4.00 hour
Moisture Content
<= 0.15 %
<= 0.15 %
Back Pressure
0.172
-
0.689
MPa
25.0
-
100
psi
Screw Speed
25
-
75
rpm
25
-
75
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PSTARP9801 / 254987
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.