MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Natural Rubber, Vulcanized (NR, IR, Polyisoprene)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Natural rubber is polyisoprene. Chemical and environmental resistance and mechanical properties are improved through crosslinking (vulcanizing), usually through treatment with sulfur.

Natural rubber usually withstands polar organic solvents (alcohols, ketones, aldehydes), organic acids, and mild chemicals. Its is adversely affected by most hydrocarbons, oil/grease/fat, strong acid, and ozone.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccUncompounded
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 30 - 100Depends on compounding
Hardness, Shore D 30 - 45Depends on compounding
Tensile Strength, Ultimate 28.0 MPaCompounded Tire
Elongation at Break 100 - 800 %
100% Modulus 0.00150 GPa
@Strain 100 %
Shear Modulus 0.000500 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+16 ohm-cm
Dielectric Constant 2.9
@Frequency 1000 Hz
Dielectric Strength 50.0 kV/mmStep by step
Dissipation Factor 0.0020
@Frequency 60.0 - 1000 Hz
 0.030
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 225 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 0.440 J/g-°C
Thermal Conductivity 0.150 W/m-K
Maximum Service Temperature, Air 80.0 °C
Minimum Service Temperature, Air -55.0 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.526

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Natural Rubber, Not Vulcanized (NR, IR, Polyisoprene)
Overview of materials for Silicone Rubber
ATG s.r.l. NR Natural Rubber
Butyl Rubber (IIR, CIIR, BIIR)
Metflex EM67 Natural Rubber

P0RUB1 / 20064

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.