MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Toyobo T-750 Nylon, Painting Grade
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Key Feature: Glass fiber and mineral reinforced, high heat distortion grades

Information provided by Toyobo Co., Ltd

Key Words: Polyamide; Toyobo Company
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.45 g/cc0.0524 lb/in³ASTM D792
Water Absorption 0.70 %0.70 %ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm
@Thickness 3.00 mm
0.0030 in/in
@Thickness 0.118 in
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
@Thickness 3.00 mm
0.0080 in/in
@Thickness 0.118 in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM D785
Tensile Strength, Ultimate 123 MPa17800 psiASTM D638
Elongation at Break 3.8 %3.8 %ASTM D638
Modulus of Elasticity 7.20 GPa1040 ksiASTM D638
Flexural Yield Strength 183 MPa26500 psiASTM D790
Flexural Modulus 7.20 GPa1040 ksiASTM D790
Izod Impact, Notched 1.20 J/cm2.25 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Dielectric Strength 22.0 kV/mm
@Thickness 2.00 mm
559 kV/in
@Thickness 0.0787 in
ASTM D149
Arc Resistance 120 sec120 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear 43.0 µm/m-°C
@Temperature 20.0 °C
23.9 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 217 °C423 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 203 °C397 °FASTM D648
Flammability, UL94 HBHBunregistered

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Toyobo T-422-02R Nylon, Mineral-Reinforced
Toyobo T-400 Nylon, 15% Glass-Reinforced
Toyobo GLAMIDE® TY-791GT 6T-Nylon
Toyobo GLAMIDE® T-808-02 Nylon-6
Toyobo GLAMIDE® T-779 Nylon-6

PTOY48 / 70720

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.