MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Elvanol® 40-05 Polyvinyl Alcohol Specialty and Adhesive Grade  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Film

Material Notes: Elvanol® polyvinyl alcohol (PVOH) is used in the manufacture of spiral wound tubes, coated paper and linerboard, and specialty water-soluble films. Its higher binding capacity versus synthetic latex and starch make it attractive for use in coatings. It adds strength in recycle board and adds barrier properties for improved oil and grease resistance.

Applications:

  • Silicone release
  • Oil and grease resistance
  • Label stock pigment coating
  • Fluorochemical extender
  • Strengthening recycle board

Water Soluble Films

Pouches and sachets manufactured with films of DuPont™ Elvanol® are water soluble, dissolving as they release their content into cold or warm aqueous solutions. Applications include water treatment chemicals, dyes, laundry detergents, agricultural chemicals, disinfectants, industrial cleaning chemicals and other areas benefiting from ready-to-use, pre-measured dosages or reduced packaging waste.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
pH 5.0 - 7.0
Viscosity 5.0 - 6.0 cP
@Temperature 20.0 °C
4% solids aqueous solution, Hoeppler falling ball method
Ash <= 0.50 %Dry basis calculated as % Na2O
Collected Volatile Condensable Material <= 5.0 %
 
Descriptive Properties
Hydrolysis72-76%Mole % hydrolysis of acetate groups, dry basis

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Elvanol® 51-03 Polyvinyl Alcohol Partially Hydrolyzed General Purpose Grade
DuPont Elvanol® 85-91 Polyvinyl Alcohol Specialty and Adhesive Grade
DuPont Elvanol® 51-04 Polyvinyl Alcohol Partially Hydrolyzed General Purpose Grade
DuPont Elvanol® 75-15 Polyvinyl Alcohol Specialty and Adhesive Grade
DuPont Elvanol® T-25 Polyvinyl Alcohol Textile Grade

PDUPM095 / 33762

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.