MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Cray Valley Wingtack® RWT 7850 Aliphatic C-5 Hydrocarbon Resin
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: Wingtack® RWT 7850 is a light yellow, aliphatic hydrocarbon resin that promotes a higher softening point, and very good color and viscosity stability at compounding temperatures.

Product Highlights / Performance Properties:

  • Good compatibility with waxes, olefins, EVA, and less-polar polymers typically used in adhesives and coatings
  • Generally soluble in solvents having low to medium polarity
  • Elastomer compatibility including EPDM
Suggested Applications:
  • Hot melt adhesives (HMA)
  • Pressure sensitive adhesives (PSA)
  • Sealants
  • Plastics & Rubber

Information provided by Cray Valley

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.950 g/cc0.950 g/ccASTM D891
Molecular Weight 1000 g/mol1000 g/molMn
 2100 g/mol2100 g/molMw
Ash 0.00 %0.00 %
 
Thermal PropertiesMetricEnglishComments
Softening Point 102 °C216 °FE-950
Glass Transition Temp, Tg 56.0 °C133 °Fmidpoint
 
Optical PropertiesMetricEnglishComments
Gardner Color Number 2.12.1in 50% toluene; E-803
 
Descriptive Properties
AppearanceYellow
Clarity0.955E-803a

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCRAYV037 / 316190

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.