MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
American Beech Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Hardwood. Least easy to work with hand tools. Very good steam bending, fair shaping. Data is based on small, clear, air-dried samples unless specified.

Property values marked by an asterisk (*) have been taken from an unusually old reference source.

Key Words: Fagus grandifolia; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.560 g/ccOven Dry Weight/Unseasoned Volume
 54.0 lb/ft³Unseasoned*
Cell Length 1.20 mmMature Wood
 
Mechanical PropertiesOriginal ValueComments
Hardness, Wood Indentation 3600 NSide. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 4200 NEnd. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 5800 NSide
Tensile Strength, Ultimate 7.00 MPaPerpendicular to Grain
 760 psiPerpendicular to Grain*
Modulus of Rupture 0.103 GPaIn Bending
 8.20 ksiStatic Bending*
Flexural Yield Strength 60.0 MPaBending stress at proportional limit
 4500 psiFiber Stress at Elastic Limit; Static Bending*
Flexural Modulus 11.7 - 11.9 GPaIn Bending
 1240 ksiStatic Bending*
Compressive Strength 7.00 MPaPerpendicular to Grain
 50.0 - 50.3 MPaParallel to Grain
 610 psiPerpendicular to Grain*
 2550 psiParallel to Grain*
 3280 psiMax Crushing Strength Parallel to Grain*
Shear Strength 13.9 MPaOrientation Unknown
 1210 psiParallel to Grain*
Impact 4.2in-lb/in³; Work to Elastic Limit; Unseasoned Sample; Impact Bending*
 10400psi; Fiber Stress at Elastic Limit; Unseasoned Sample; Impact Bending*
Work to Elastic Limit 0.990 in-lb/in³Static Bending*
Work to Maximum Load 12.5 in-lb/in³Static Bending*
Cleavage 59.0 kN/mRadial surface of failure, Unseasoned*
 92.0 kN/mTangential surface of failure, Unseasoned*
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.40 µm/m-°C
@Temperature 20.0 °C
Axial. Typical value for Beech.
 22.0 µm/m-°C
@Temperature 20.0 °C
Radial; Typical value for Beech.
 34.8 µm/m-°C
@Temperature 20.0 °C
Tangential. Typical value for Beech.
Specific Heat Capacity 0.390 J/g-°CWhite Oak
Thermal Conductivity 0.173 W/m-KWhite Oak
 1.00 BTU-in/hr-ft²-°FOven Dry
 1.30 BTU-in/hr-ft²-°F12% Moisture Content
Shrinkage 5.1 %Radial; Green to Zero Moisture
 11 %Tangential; Green to Zero Moisture
 16.3 %Volumetric; Green to Zero Moisture

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
European Beech Wood
American Yellow Birch Wood
American Maple, Rock (Sugar Maple)
American White Oak Wood
American Ash Wood

PTSAO / 71298

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.