MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECACOMP POM AH blue 1018432 POM-C
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes:
  • food grade blue
Target Industries:
  • food engineering

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³
Melt Flow 3.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.2 g/10 min
@Load 4.76 lb,
Temperature 374 °F
DIN EN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 55.0 MPa7980 psi50 mm/min; DIN EN ISO 527-1
Elongation at Break 62 %62 %50 mm/min; DIN EN ISO 527-1
Modulus of Elasticity 2.40 GPa348 ksi50 mm/min; DIN EN ISO 527-1
Charpy Impact Unnotched 15.0 J/cm²71.4 ft-lb/in²DIN EN ISO 179-1eU
 
Thermal PropertiesMetricEnglishComments
Melting Point 165 °C329 °FDIN 53765
Maximum Service Temperature, Air 100 °C212 °Flong term
 140 °C284 °Fshort term
Glass Transition Temp, Tg -60.0 °C-76.0 °FDIN 53765
 
Processing PropertiesMetricEnglishComments
Processing Temperature 170 - 230 °C338 - 446 °FCylinder
Melt Temperature 210 - 230 °C410 - 446 °FMaterial temperature
Mold Temperature 80.0 - 140 °C176 - 284 °F
Drying Temperature 100 - 120 °C212 - 248 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
 
Descriptive Properties
Colorblue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIO9109 / 319037

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.