MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Bakelite® UP 3620 Unsaturated Polyester Resin, High Surface Quality, UL Listed
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: Polyester molding compound, mainly organically filled, styrene free, processing shrinkage as for phenolic molding compounds, non flammable, high surface quality, UL listed molding compound 1,5 mm / V-0 (ALL).

Applications: Lamp parts, switch gears, housings and base plates, MCB housings.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.71 g/ccISO 1183
Apparent Bulk Density 0.700 g/ccISO 60
Linear Mold Shrinkage 0.0070 cm/cmCompression Molding. Post Shrinkage = 0.25%.; ISO 2577
 0.0075 cm/cmInjection Molding. Post Shrinkage = 0.25%.; ISO 2577
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 250 MPaH961/30; ISO 2039/P1
Tensile Strength 50.0 MPaISO 527 - 1/2
Tensile Modulus 8500 MPaISO 527 - 1/2
Flexural Strength 80.0 MPaISO 178
Flexural Modulus 7500 MPaISO 178
Compressive Strength 180 MPaISO 604
Charpy Impact Unnotched 7.50 kJ/m²ISO 179-1 eU
Charpy Impact, Notched 1.90 kJ/m²ISO 179-1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cm
Surface Resistance 1.00e+11 ohm
Dielectric Constant 5.0
@Frequency 100 Hz
Dielectric Strength 30.0 kV/mm
@Thickness 1.00 mm
IEC 60243-P1
Dissipation Factor 0.020
@Frequency 100 Hz
Arc Resistance 140 - 145 secASTM D495
High Voltage Arc Resistance to Ignition (HVAR) >= 300 sec
@Thickness 1.50 mm
(ALL)
Comparative Tracking Index 600 V
Hot Wire Ignition, HWI 60 - 120 sec
@Thickness 1.50 mm
(ALL)
 >= 120 sec
@Thickness 3.00 mm
ALL
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 1.50 mm
(ALL)
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min
@Thickness 3.00 mm
ALL
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 130 °C<20000 hours; IEC 60216-P1
 190 °C< 50 hours; IEC 60216-P1
Deflection Temperature at 8.0 MPa 70.0 °CISO 75-2
UL RTI, Electrical 105 °C
@Thickness 1.50 mm
(ALL)
UL RTI, Mechanical with Impact 130 °C
@Thickness 1.50 mm
(ALL)
UL RTI, Mechanical without Impact 130 °C
@Thickness 1.50 mm
(ALL)
Flammability, UL94 V-0
@Thickness 1.50 mm
All colors
 
Processing PropertiesOriginal ValueComments
Feed Temperature 60.0 - 70.0 °CInjection molding
Nozzle Temperature 70.0 - 100 °CInjection molding
Melt Temperature 70.0 - 100 °CInjection molding
Mold Temperature 160 - 180 °CInjection molding
 160 - 180 °CCompression molding
Injection Pressure >= 10.0 MPaCompression and injection cavity mold pressure
Back Pressure 0.500 - 1.00 MPaInjection molding
Cure Time 10.0 - 20.0 secPer 1 mm of wall thickness, injection molding
 20.0 - 40.0 secPer 1 mm of wall thickness, compression molding
 
Descriptive Properties
Creep Rupture StrengthMedium
Holding PressureApproximately 40-60% of injection pressure
Media ResistanceMedium
Thermal ExpansionSlight
Water absorption (mg)7024h / 23°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bakelite® UP 3415 Unsaturated Polyester Resin, Low Shrinkage, High Arc Resistance, UL Listed, High Mechanical Strength
Bakelite® UP 3420 Unsaturated Polyester Resin, High Mechanical Strength, High Arc Resistance, UL Listed, Low Shrinkage
Bakelite® UP 804 Unsaturated Polyester Resin, High Surface Quality, UL Listed, Low Shrinkage, High Arc Resistance
Bakelite® UP 3720 Unsaturated Polyester Resin, UL Listed, Low Shrinkage, High Arc Resistance
Bakelite® UP 802 Unsaturated Polyester Resin, High Surface Quality, Low Shrinkage, High Arc Resistance

PBAKE055 / 27089

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.