MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Elvax® 40L-03 Ethylene-Vinyl Acetate Copolymer Resin
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Wire/Cable Grade

Material Notes: Elvax® 40L-03 is an ethylene-vinyl acetate copolymer that is useful in many wire and cable applications because of its excellent mechanical, thermal, and low-smoke properties. The melt index is appropriate for convenient compounding and extrusion. The melt index is consistent because resin molecular weight distribution is controlled to within a relatively narrow range. The molecular weight is high, so finished products will be relatively resistant to mechanical damage and elevated temperatures.

Compared with other ethylene-vinyl acetate copolymers, Elvax® 40L-03 contains extremely low amounts of gel, or high molecular weight polymer, that can cause undesirable characteristics in finished products

Because Elvax® 40L-03 is somewhat crystalline, it is free flowing and does not mass during handling.

Typical Applications:

  • Jacketing compounds for automotive ignition and low-smoke cables
  • Strippable semiconductive shields for power cables

Features:

  • Narrow molecular weight distribution and low gel properties for consistent and smooth surfaced finished products
  • Stable, long-term cable performance

Information provided by DuPont.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.968 g/ccASTM D1505
Vinyl Acetate Content 40 %DuPont Method
Melt Index of Compound 2.1 - 3.9 g/10 minASTM D1238-82
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 52ASTM D2240-81
Tensile Strength at Break 9.80 MPaASTM D882-83
Elongation at Break 980 %ASTM D882-83
 
Descriptive Properties
Vinyl Acetate Content40 wt.%DuPont Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema EVATANE® 40-55 Copolymer Ethylene - Vinyl Acetate
Dow Elvax® 260 Ethylene-Vinyl Acetate Copolymer Resin
Arkema Evatane® 1003 VL 2 Ethylene Vinyl Acetate
Dow Elvax® 40W Ethylene-Vinyl Acetate Copolymer Resin
Arkema EVATANE® 42-60 Copolymer Ethylene - Vinyl Acetate

PDUPM112 / 33779

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.