MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ascend Performance Materials Vydyne® 88X Nylon 66/6 Compounding Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Vydyne 88X is a medium-viscosity PA66/6 random copolymer used for extrusion-compounding. It provides benefits for compounds containing heat-sensitive additives and for end applications that require good surface finish. This copolymer is specifically designed to be used with FR packages and high mineral loadings. Vydyne 88X is the product of choice for low-yellowness-required applications. Vydyne 88X maintains the chemical resistance typical of PA66/6 to many chemicals, machine and motor oils, solvents and gasoline.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.674 g/cc0.0243 lb/in³ASTM D1895
Density 1.14 g/cc0.0412 lb/in³ISO 1183
Moisture Absorption 0.500 %0.500 %ASTM D6869
Viscosity Measurement 45 - 5145 - 51Relative Viscosity - Formic acid; ASTM D789
Viscosity Test 137 - 148 cm³/g1.37 - 1.48 dl/gViscosity Number (H2SO4, sulfuric acid); ISO 307
 
Thermal PropertiesMetricEnglishComments
Melting Point 255 °C491 °FISO 11357-3
 
Optical PropertiesMetricEnglishComments
Yellow Index -4.00 %-4.00 %ASTM D1925
 
Descriptive Properties
FeaturesCopolymer
 Gasoline Resistance
 General Purpose
 Good Abrasion Resistance
 Good Chemical Resistance
 Good Toughness
 High Rigidity
 High Strength
 Oil Resistant
 Solvent Resistant

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PZASCE9916 / 220966

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.