MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sylvania SX276 Molybdenum Thermal Spray Powder
Categories: Ceramic; Carbide; Metal; Nonferrous Metal; Molybdenum Alloy; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: General Description

SX276 is a spherical agglomerate of molybdenum and molybdenum carbide particles. The powders are spherical and free flowing and can be applied by plasma or high velocity thermal spray processes. These coatings can be used for adhesive and abrasive wear-resistance in a variety of industrial applications.

Applications

  • Coating on screws for plastic processing
  • Piston and synchronizer ring coatings
  • Steel mill machinery

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 2.00 - 4.30 g/cc
Particle Mesh Size 170 Mesh2.5% bigger
 325 Mesh20% smaller
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 1.8 - 2.4 %
Molybdenum, Mo 97.6 - 98.2 %
 
Descriptive Properties
Hall Flow, seconds/50g30-40ASTM B213

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sylvania SD254 Tungsten & Chrome Based Thermal Spray Powder
Sylvania SX158 Tungsten & Chrome Based Thermal Spray Powder
Aluminum 6061-T6; 6061-T651
Sylvania SD152 Molybdenum Thermal Spray Powder
AISI Type A11 Tool Steel (UNS T30111)

CSYLV07 / 2306

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.