System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Samyang Trimma® FT6120 I[R] PMMA, Transparent
Categories:
Polymer
;
Thermoplastic
;
Acrylic (PMMA)
;
Acrylic, Optical Grade, Molded
Material Notes:
High transparency and high scratch resistance. Stable against weak acids, strong acids, weak alkalis and inorganic salts.
Applications:
Laptop, Monitor Front Cover - for high flow, high gloss and high hardness
Information provided by Samyang.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.18
g/cc
ASTM D792
Linear Mold Shrinkage
0.0040
-
0.0080
cm/cm
ASTM D955
Melt Flow
8.0
g/10 min
ASTM D1238
Mechanical Properties
Original Value
Comments
Tensile Strength
750
kg(f)/cm²
ASTM D638
Elongation at Break
20 %
ASTM D638
Flexural Yield Strength
970
kg(f)/cm²
ASTM D790
Flexural Modulus
24500
kg(f)/cm²
ASTM D790
Izod Impact, Notched
2.40
kg-cm/cm
@Thickness 3.17 mm
ASTM D256
Thermal Properties
Original Value
Comments
Deflection Temperature at 1.8 MPa (264 psi)
83.0
°C
ASTM D648
Flammability, UL94
HB
@Thickness 1.50 mm
Optical Properties
Original Value
Comments
Transmission, Visible
90 %
transparent; thickness not quantified
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Samyang Trimma® SD6310H PMMA, Translucent
Hippe PMMA
Samyang Trimma® SD6350H PMMA, Opaque
Samyang Trimma® SD6320P PMMA, Translucent
Samyang Trimma® SD6320 PMMA, Translucent
PSANX959 / 133353
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.