MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Shakespeare Isocor™ TT65SI Nylon 6 Terpolymer
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Isocor™ TT65SI multi-polymer is a linear polyamide with unique solubility characteristics and physical properties. Unlike conventional polyamides, Isocor™ TT65SI is soluble in common alcohols or in alcohol/water mixtures. Isocor™ TT65SI is easily processed and has a wide range of applications due to its physical properties, chemical resistance, and lower melt temperatures.

Used for thread bonding, specialty coatings, pigment carriers, polymer additives, and specialty adhesives.

Information provided by Shakespeare Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccASTM D 792
Water Absorption 3.1 %24 hour immersion; ASTM D 570
Viscosity Measurement 65Relative Viscosity
 
Thermal PropertiesOriginal ValueComments
Melting Point 143 °CDSC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Shakespeare Isocor™ 651 Nylon 6 Terpolymer
Shakespeare Isocor™ 637 Nylon 6 Terpolymer
ExxonMobil ESCOR™ AT 310 Extrusion Coating Resin
Shakespeare Isocor™ TT25TI Nylon 6 Terpolymer
Tra-Con Tra-Bond 2143D Medium Viscosity Polyamide Epoxy Adhesive

PSHAKE103 / 67382

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.