MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Akrochem AKROSORB™ 19474 (72% TBEP) Dispersion
Categories: Other Engineering Material

Material Notes: Product Description: Akrosorb 19474 is a dry powdered dispersion of TBEP (tributoxyethyl phosphate) absorbed on a synthetic calcium silicate. This powdered form offers the compounder an easier, more accurate means of handling and weighing liquid products.

Applications: TBEP is an excellent low temperature plasticizer and softener for many synthetic elastomers, most prevalently NBR. This plasticizer helps retain high tensile strength and elongation with low hardness. TBEP offers some flame resistance and incorporates readily into compounds.

Advantages: Dry liquid dispersions (DLDs) are a proven means of upgrading plant safety, efficiency, quality and raw material control. Akrochem dry liquid dispersions eliminate the messiness of weighing liquids, as well as other potential hazards in handling liquids in the plant. The “dry” physical form is easy to handle and weigh accurately. With a dispersion, better, uniform mixing, at lower processing temperatures is possible.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.21 g/cc
 
Descriptive Properties
Active0.72
Appearanceoff-white to grey powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH144 / 315062

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.