MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemical Concepts Chem-Set™ C-20 Seaming Adhesive
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: ChemSet C-20 Seaming/Surfacing adhesive is for color matched adhesives for the surfacing industry. Available in more than 100 pre-mixed colors; developed for demanding fabrication methods such as laminating, mitering, integral mounted sinks and bowls, and applications subject to dynamic loads. ChemSet C-20 produces improved bond strength over competitor products. Fabricators benefit from increased color choices as C-20 is used universally on Acrylic and Polyester Solid Surface materials as well as Granite, Marble, Quartz Surfaces, Ceramics and more.

Applications: Quartz Surfaces, Silestone, Caesarstone, Cambria, Okite, etc., Natual Stones, Granite, Marble, Limestone, etc, Solid Surfaces, Corian, Staron, LG Hi-Macs. Avonite.

Advantages: Auto-dispense system, Eliminates hand-mixing, Invisible seams 300+ pre-mixed colors, High strength, UV stable, Working time 12 minutes, Fixture time 25 minutes, Indoor Air Quality Certified, LEED Certification Compliant.

Information provided by Chemical Concepts™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.40 lb/galAdhesive, uncured
 8.60 lb/galmixed. Room temperature cure
 9.00 lb/galActivator, uncured
pH 4.0 - 6.0adhesive
 4.0 - 6.0activator
Viscosity 15000 - 25000 cPAdhesive, uncured
 15000 - 25000 cPActivator, uncured
Vapor Pressure <= 0.500 torr
@Temperature 20.0 °C
Activator
 28.0 torr
@Temperature 20.0 °C
Adhesive
 
Mechanical PropertiesOriginal ValueComments
Adhesive Bond Strength 2500 - 3000 psiAcrylic solid surface: substrate. Failure type: cohesive; ASTM D638
 2500 - 3000 psiPolyester solid surface substrate. Failure type: substrate; ASTM D638
 
Thermal PropertiesOriginal ValueComments
Melting Point -54.0 °Fadhesive
Boiling Point 212 °Fadhesive
 >= 550 °Factivator
Flash Point 51.0 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 65.0 - 85.0 °Froom temperature cure
Working Life 10.0 - 15.0 min
@Temperature 22.2 °C
 
Descriptive Properties
AppearanceLiquid (activator)
Auto Ignition Temperature790°F (adhesive)
Chemical ResistanceAcids and bases: excellent
 Hydrocarbons: excellent
 Most household foods: excellent
 Polar solvents: susceptible
 Super strong acids and bases: susceptible
 Vinegar: excellent
 Wine and Condiments: excellent
Colorclear/various colors: Adhesive. Uncured
 Creamy white/white paste: Activator. Uncured
Evaporation Point<1 (activator)
 3 (adhesive)
Fixture Time20 to 30 minutes. Room temperature cure.
Gap Filling0.125 inches- for countertops. Room temperature cure
Mix Ratio10:1
Odormild sweet (activator)
 mild sweet (adhesive)
Routable35 to 45 minutes. Room temperature cure.
Vapor Density3.5 (air=1) adhesive

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHEMI932 / 232184

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.