MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Parker Chomerics CHO-SHIELD® 576 Platable Silver Epoxy Coating
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: Description: CHO-SHIELD® 576 coating is a two component, silver filled, highly conductive epoxy paint designed to provide EMI shielding when applied to a dielectric plastic substrate. This coating was specifically developed as a variant of CHO-SHIELD® 596. CHO-SHIELD® 576 dries to the touch in less than 1 hour at room temperature and attains full chemical resistance after 1 week at room temperature. However, the best electrical properties are achieved by curing at elevated temperatures.

Performance: CHO-SHIELD® 576 is first sprayed onto plastic substrate, and further plating operations may follow. The full stack up of plating and coating will meet strict adhesion requirements, equivalent to ASTM D3359 with a rating of 5A after exposure to 95% RH at 65°C for 24 hours and thermal cycling from one hour at -57°C to one hour at 95°C for a total of four cycles.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.80 g/cc1.80 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 40 - 6040 - 60ASTM D676
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.060 ohm-cm
@Temperature 24.0 °C,
Time 3600 sec
0.060 ohm-cm
@Temperature 75.2 °F,
Time 1.00 hour
[ohm/sq], followed by 1 hour at 121°C
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 min
@Temperature 23.8 °C
1.00 hour
@Temperature 74.8 °F
and 1 hour at 121°C
 60.0 min
@Temperature 23.8 °C
1.00 hour
@Temperature 74.8 °F
and 6 hours at 65.5°C
 120 min
@Temperature 24.0 °C
2.00 hour
@Temperature 75.2 °F
and 45 minutes at 65.5°C, followed by 45 minutes at 98.8° C (recommended)
 10100 min
@Temperature 23.8 °C
168 hour
@Temperature 74.8 °F
Pot Life 480 min480 min
Shelf Life 9.00 Month9.00 Month
 
Descriptive Properties
Suggested Spraying Viscosity #2 Zahn Cup15 sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHOME234 / 130944

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.