MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Victrex VICOTE™ 705 Black Polyetheretherketone (PEEK) Powder Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Polyketone; Polyetheretherketone (PEEK)

Material Notes: VICOTE™ 705Blk is a black pigmented version of the 705 grade. This grade has a nominal particle size of about 50 microns. The powder is dark grey in colour and is a low melt viscosity grade for lower film builds. Typical film thicknesses range from 50 - 80 microns. The final coating takes on a dark gun metal grey colour after stoving.

VICOTE Coatings, like other noncoating grades of VICTREX PEEK polymer, are thermoplastic in nature and exhibit flow above the melt temperature. When processed using the correct guidelines the coatings will exhibit the excellent properties that VICTREX PEEK polymer is renowned for.

Typical properties are high continuous use temperature of 260°C, excellent wear, abrasion and cut through resistance at these high temperatures combined with excellent chemical and radiation resistance. VICOTE Coatings have a low level of extractables and are hydrolysis resistant and inherently flame retardant. Meets FDA 21 CFR 175.300

Information Provided by Victrex.

Vendors: Victrex is a global leader in high-performance PEEK and PAEK polymers, transforming industries from aerospace to medical devices. For 40 years, our innovative polymer solutions help customers achieve new levels of performance, sustainability, and cost efficiency across applications that millions rely on daily from smartphones to aircraft components. As pioneers in polymer engineering, we're committed to delivering transformational solutions that address global materials challenges. Visit www.victrex.com, call (800) VICTREX /1-484-342-6001, or email victrexplc@victrex.com.

Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.32 g/ccISO 1183
 
Thermal PropertiesOriginal ValueComments
Melting Point 343 °CDSC
Maximum Service Temperature, Air 260 °C
Glass Transition Temp, Tg 143 °CDSC
UL RTI, Electrical 260 °CUL 746B
UL RTI, Mechanical with Impact 260 °CUL 746B
UL RTI, Mechanical without Impact 260 °CUL 746B
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
Konig Hardness (seconds)200Test Method: BS EN ISO 1522

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SK Chemicals SKYTHANE® UB410 Powder Coating
Avient Edgetek® AS-20CF/000 Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced
Avient Edgetek® AS-13CF/000 Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced
Eurotec® Tecomid® NB30 BK EF PA6, unfilled, black, suitable for electrostatic powder coating
Eurofoam Porocell POR 304 B EPDM Foam

PVICTA79 / 99757

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.