MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
ALM PA 850 Black Nylon 11 SLS Prototyping Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 11 (PA11)

Material Notes:

Information provided by Advanced Laser Materials (ALM).

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Bulk Density 0.500 g/ccASTM D1895
Density 1.03 g/ccSintered Part; ASTM D792
Particle Size 50 µmAverage D50; Laser Diffraction
 38 - 78 µmRange (D10 to D90); Laser Diffraction
Melt Flow 26 g/10 min
@Load 5.00 kg,
Temperature 235 °C
3 min.; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 74ASTM D2240
Tensile Strength at Break 48.0 MPaXY direction; ASTM D638
Tensile Strength, Ultimate 42.0 MPaZ direction; ASTM D638
Elongation at Break 14 %Z direction; ASTM D638
 51 %XY direction; ASTM D638
Tensile Modulus 1.43 GPaZ direction; ASTM D638
 1480 MPaXY direction; ASTM D638
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.3e+13 ohm-cm50% RH; 500V; ASTM D257
Surface Resistance 4.9e+12 ohm50% RH; 500V; ASTM D257
 
Thermal PropertiesOriginal ValueComments
CTE, linear 120 µm/m-°C
@Temperature 0.000 - 50.0 °C
ASTM E831
 342 µm/m-°C
@Temperature 85.0 - 145 °C
ASTM E831
Melting Point 200 °CASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 188 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 48.0 °CASTM D648
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ALM PA 850-Nat Nylon 11 SLS Prototyping Polymer
ALM PA 650 Nylon 12 SLS Prototyping Polymer
CRP Technology Windform® RL Thermoplastic Elastomer for SLS
ALM D80-ST Nylon 11 SLS Prototyping Polymer
ALM PA 860 White Nylon 11 SLS Prototyping Polymer

PALAP97 / 176027

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.