MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röhm ACRYLITE® Soundstop NT Acrylic based polymer  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Product: ACRYLITE® Soundstop NT CC is a highly filled, non-transparent grade of cast acrylic.

Properties: In addition to the well-known and proven properties of ACRYLITE®, such as

  • extremely high weather resistance
  • ease of fabrication
  • high surface hardness
  • low weight
  • 100% recyclability,
ACRYLITE® Soundstop NT offers the following special features:
  • Large noise barrier elements reduce the need for steel supporting structures.
  • ACRYLITE® Soundstop NT achieves the highest airborne sound reduction category (B3) of EN 1793-2, and also meets all requirements of EN 1794-1,2.
  • ACRYLITE® Soundstop NT is available in various colors.
  • ACRYLITE® Soundstop NT can be supplied with a matte or gloss surface.
  • Since the sheets are homogeneously colored, there is no flaking.
Applications: These properties make ACRYLITE® Soundstop NT especially suitable for
  • noise control along roads and railways
  • wind barriers on bridges

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm (Roehm) GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.67 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 37.0 MPaISO 527-2/1B/5
Elongation at Break 2.0 %ISO 527-2/1B/5
Modulus of Elasticity 7.20 GPaISO 527-2/1B/5
Flexural Strength 62.0 MPaISO 178
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µin/in-°FDIN 53752-A
Maximum Service Temperature, Air 70.0 °C
Vicat Softening Point 105 °CISO 306-B50

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Röhm Acrylite Plus® zdf Impact Acrylic Polymer
Röhm Acrylite Plus® zk3HR Impact Acrylic Polymer
Röhm Acrylite Plus® zk4BR Impact Acrylic Polymer
Röhm Acrylite Plus® zk4HR Impact Acrylic Polymer
Röhm Acrylite Plus® zk5BR Impact Acrylic Polymer

PEVONIL083 / 196287

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.