MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

BYK Pure Thix® 1442 Associative Thickener for Water or Water Phase for Personal Care
Categories: Ceramic; Clay; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: PURE THIX 1442 is a flake that forms a clear aqueous solution of a nonionic hydrophobe modified polymer (INCI name: Polyether-1) designed especially for thickening the water phase of personal care formulations. PURE THIX 1442 will be listed on the next EPS Inert List published.

Application:

  • Lotions Bath and shower gels
  • Liquid cleansers and soaps Hair care
  • Sunscreen products Make-up

Information provided by Southern Clay Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 100 %100 %
pH >= 5.5>= 5.5
Viscosity  40 cP
@Temperature 88.0 °C,
Time 1800 sec
40 cP
@Temperature 190 °F,
Time 0.500 hour
 60 cP
@Temperature 60.0 °C,
Time 3600 sec
60 cP
@Temperature 140 °F,
Time 1.00 hour
 65 cP
@Temperature 40.0 °C,
Time 10800 sec
65 cP
@Temperature 104 °F,
Time 3.00 hour
 70 cP
@Temperature 24.0 °C,
Time 32400 sec
70 cP
@Temperature 75.2 °F,
Time 9.00 hour
 
Descriptive Properties
Color/FormDry Flakes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BYK Optigel® WH Clay Additive
BYK Optigel® WA Clay Additive
BYK Optigel® W724 Thickener
BYK Optigel® LX Clay Additive
BYK Optigel® CMO Thickener

PBYK109 / 185106

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.