MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Aremco Aremco-Bond™ 2315X High Temperature Epoxide Potting Compound
Categories: Polymer; Thermoset; Epoxy; Epoxy, High Temperature

Material Notes: Improved Crack Resistance & Bond Strength. High Temperature Resistance, Thermally Conductive, Low Viscosity.

Vendors: Aremco’s High Performance Epoxies provide a wide range of solutions for bonding ceramics, composites, glass, metals, plastics, and other materials. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Aremco

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.95 g/cc
Viscosity 4000 cPMixed
Linear Mold Shrinkage 0.0030 in/incure shrinkage
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 92
Flexural Strength 12300 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cm
Dielectric Constant 4.7
@Frequency 1000 Hz
Dielectric Strength 480 V/mil
Dissipation Factor 0.010
 
Thermal PropertiesOriginal ValueComments
CTE, linear 19.0 µin/in-°F
Thermal Conductivity 8.40 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 365 °F
Minimum Service Temperature, Air -67.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 71.1 °C
Step 1 of recommended 2 step cure
 2.00 hour
@Temperature 149 °C
Step 2 of recommended 2 step cure
 4.00 hour
@Temperature 104 °C
Alternate
Pot Life >= 480 min
@Temperature 25.0 °C
100 gm mass
 
Descriptive Properties
Chemical ResistanceExcellent
ColorBlack
Mix Ratio100:25

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trelleborg Emerson & Cuming Stycast® 2762/17M-1 Two-Component Epoxy High Service Temp Encapsulant
Trelleborg Emerson & Cuming Stycast® 4952/25 Two-Component Silicone High Service Temp Encapsulant
Trelleborg Emerson & Cuming Stycast® W-66/17M-1 Two-Component Epoxy High Service Temp Encapsulant
Abatron AboCast/AboCure 8501-4/8501-4 High Temperature Resistant Epoxy
Abatron AboCast/AboCure 50-7/8501-4 High Temperature Resistant Epoxy

PAREM08e / 178189

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.