MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

SABIC ULTEM™ Resin SF2350 Polyetherimide (PEI) (Europe)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: High flow ULTEM blends for thin wall application

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.52 g/cc1.52 g/ccASTM D792
Density 1.52 g/cc0.0549 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Viscosity 30 cP
@Load 10.0 kg,
Temperature 345 °C
30 cP
@Load 22.0 lb,
Temperature 653 °F
MVR cc/10 min; ISO 1133
Melt Flow 14.7 g/10 min
@Load 6.60 kg,
Temperature 337 °C
14.7 g/10 min
@Load 14.6 lb,
Temperature 639 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 171 MPa24800 psi5 mm/min; ISO 527
 172 MPa24900 psi5 mm/min; ASTM D638
Elongation at Break 2.5 %2.5 %5 mm/min; ISO 527
 2.6 %2.6 %5 mm/min; ASTM D638
Tensile Modulus 11.6 GPa1680 ksi5 mm/min; ASTM D638
Flexural Strength 222 MPa32200 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 9.32 GPa1350 ksi1.3 mm/min, 50 mm span; ASTM D790
 9.40 GPa1360 ksi2 mm/min; ISO 178
Izod Impact Notched 95.0 J70.1 ft-lbASTM D256
Izod Impact, Notched (ISO) 10.0 kJ/m²4.76 ft-lb/in²80*10*4; ISO 180/1A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  14.0 µm/m-°C
@Temperature 23.0 - 150 °C
7.78 µin/in-°F
@Temperature 73.4 - 302 °F
ISO 11359-2
 15.0 µm/m-°C
@Temperature -40.0 - 150 °C
8.33 µin/in-°F
@Temperature -40.0 - 302 °F
ASTM E831
CTE, linear, Transverse to Flow  55.0 µm/m-°C
@Temperature -40.0 - 150 °C
30.6 µin/in-°F
@Temperature -40.0 - 302 °F
ASTM E831
 56.0 µm/m-°C
@Temperature 23.0 - 150 °C
31.1 µin/in-°F
@Temperature 73.4 - 302 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 209 °C408 °FEdgew 120*10*4 sp=100mm; ISO 75/Ae
 204 °C
@Thickness 3.20 mm
399 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 345 - 400 °C653 - 752 °F
Zone 2 340 - 400 °C644 - 752 °F
Zone 3 345 - 400 °C653 - 752 °F
Melt Temperature 350 - 400 °C662 - 752 °FInjection Molding
Mold Temperature 135 - 165 °C275 - 329 °F
Drying Temperature 150 °C302 °FInjection Molding
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection Molding
 24.0 hour24.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 40 - 60 %40 - 60 %
Vent Depth 0.00250 - 0.00760 cm0.000984 - 0.00299 in
Screw Speed 40 - 70 rpm40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82763 / 290710

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.