Vermiculite. Hydraulic bond. A 1100°C lightweight, low iron insulating material installed by casting, gunning or trowelling. Conforms to ASTM Class N & O. Applications: Suitable for back-up insulation in most industrial applications. Contains portland cement. Information provided by Morgan Advanced Materials |