MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Sika Sikaflex® -1c SL High performance, self-leveling, 1-part polyurethane sealant
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Sikaflex-1c SL is a single component, self-leveling, premium-grade polyurethane sealant with an accelerated curing capacity. Meets Federal Specification TT-S-00230C, Type I, Class A. Meets ASTM C-920, Type S, Grade P, Class 25, use T, M, A, G, I.

Where to Use: Sikaflex-1c SL is used to seal horizontal expansion joints in concrete and cementitious slabs such as:

  • Sidewalks
  • Balconies
  • Pavements
  • Terraces
  • Warehouses
  • Factories
  • Civil Structures
  • Plazas
  • Pitch Pans
  • Canals and Water Treatment
Advantages:
  • 1-component, no mixing
  • Self-leveling, pourable
  • Accelerated curing
  • Can be applied to green concrete 24 hours after pour
  • Can be applied to damp concrete 1 hour after getting wet
  • Extremely elastic
  • High durability
  • Resists aging, weathering
  • Excellent adhesion
  • Convenient, easy-to-use packaging
  • Jet fuel resistant
  • Water Immersion Applications

Information provided by Sika Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatile Organic Compounds (VOC) Content 40 g/l
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 35 - 4521 day; ASTM D2240
Tensile Strength 150 psi21 day; ASTM D412
Tensile Stress at Strain 110 psi
@Strain 100 %
ASTM D412
Elongation at Break 320 %ASTM D412
Peel Strength >= 28.0 pliMortar, 0% Adhesion loss; ASTM C-794
 >= 30.0 pliAluminum, 0% Adhesion loss; ASTM C-794
 >= 37.0 pliGlass, 0% Adhesion loss; ASTM C-794
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 170 °F
Minimum Service Temperature, Air -40.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 72.0 - 120 hourFinal cure
Tack-Free Time 1.00 - 2.00 hour
Shelf Life 6.00 Month
@Temperature 4.00 - 35.0 °C
4.5 gallon pail
 6.00 Month
@Temperature 4.00 - 35.0 °C
50 gallon drum
 12.0 Month
@Temperature 4.00 - 35.0 °C
10.1 fl. oz. cartridges
 12.0 Month
@Temperature 4.00 - 35.0 °C
29 oz. cartridge
 
Descriptive Properties
ColorLimestone

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSIKA937 / 209844

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.